dc.identifier.citationÖztürk, D; Şen, N; İşler, S. Effect of non-thermal plasma treatment and resin cements on the bond strength of zirconia ceramics with different yttria concentrations. Biomedical Engineering / Biomedizinische Technik(2023).en_US
dc.identifier.issn1862-278X
dc.identifier.urihttps://www.degruyter.com/document/doi/10.1515/bmt-2023-0336/html
dc.identifier.urihttps://doi.org/10.1515/bmt-2023-0336
dc.identifier.urihttps://hdl.handle.net/20.500.12780/764
dc.description.abstractObjectives: To investigate the effect of different surface treatments and resin cements on the shear bond strength of zirconia ceramics with different yttria concentrations. Methods: Zirconia blocks characterized by different yttria concentrations [Vita YZ HT (HT), Vita YZ ST (ST) and Vita YZ XT (XT)] were used to prepare disc-shaped specimens (n=252). Specimens prepared to investigate shear bond strength (SBS), water contact angle and surface roughness (Ra) were divided into four subgroups; control (C), sandblasting (S), sandblasting + nonthermal plasma treatment (SNTP) and nonthermal plasma treatment (NTP). For SBS testing, specimens were further divided into two groups (n=108) according to the luting cement used [Panavia F2.0 (P) and Rely X U200 (R)]. The water contact angles were determined by sessile drop technique and Ra was analyzed with optical profilometer. SBS tests were performed in a universal testing machine at a crosshead speed of 0.5 mm/min. The data sets were statistically analyzed with two and three-way ANOVAs followed by post-hoc comparisons (α=0.05). Results: The water contact angle and Ra data were significantly affected by surface treatments. The mean Ra values of ST and XT were significantly lower than HT for the surface treatment groups of C and NTP. The SBS values were significantly different among the groups subjected to different surface treatments. The mean SBS values of surface treatment groups (S, SNTP and NTP) when cemented with R were significantly higher than the groups of C (p<0.05). Conclusions: For the tested zirconia ceramics with different yttria concentrations, non-thermal plasma activation helps to improve SBS and is a promising tool in practical use.en_US
dc.language.isoengen_US
dc.publisherDe Gruyteren_US
dc.relation.isversionof10.1515/bmt-2023-0336en_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectPlasma activationen_US
dc.subjectShear bond strengthen_US
dc.subjectSurface treatmentsen_US
dc.subjectZirconia ceramicsen_US
dc.titleEffect of non-thermal plasma treatment and resin cements on the bond strength of zirconia ceramics with different yttria concentrationsen_US
dc.typearticleen_US
dc.contributor.departmentİstanbul Kent Üniversitesi, Fakülteler, Diş Hekimliği Fakültesi, Klinik Bilimler Bölümüen_US
dc.contributor.authorIDhttps://orcid.org/0000-0003-2768-2112en_US
dc.contributor.institutionauthorŞen, Nazmiye
dc.relation.journalBiomedical Engineering / Biomedizinische Techniken_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster